Technical Data

3200 Innovation Place
Youngstown, Ohio 44509
Phone: (800)523-4899
Fax: (330)797-7543

EMAIL

Weld Tin Plate to:

 

Weldability

Electrode
Against

Electrode
Against

Special Information

Tungsten
Molybdenum

Poor

Copper CL2

Copper CL1

Coating may dissolve in other metals or burn away.

Magnesium

Poor

Copper CL1

Copper CL1

Welding conditions must be accurately controlled
Coating may dissolve in other metals or burn away.

Nickel Alloy

Fair

Copper CL1

Copper CL1

Low weld strength. Coating may dissolve in other metals or burn away.

Nickel

Fair

Copper CL2

Copper CL1

Coating may dissolve in other metals or burn away.

Stainless Steel

Good

Copper CL2

Copper CL1

 

Chrome Plate

Good

Copper CL2

Copper CL1

Use one flat tip to minimize distortion or discoloration.

Cadmium Plate

Fair

Copper CL1

Copper CL1

Coating may dissolve in other metals or burn away.

Galvanized Iron
Zinc Plate

Good

Copper CL1

Copper CL1

Keep electrodes clean to prevent sticking to the work. Coating may dissolve in other metals or burn away.

Terne Plate

Fair

Copper CL1

Copper CL1

Keep electrodes clean to prevent sticking to the work. Coating may dissolve in other metals or burn away.

Tin Plate

Fair

Copper CL1

Copper CL1

Keep electrodes clean to prevent sticking to the work. Coating may dissolve in other metals or burn away.

BACK

HOME

NEXT